All of the following statements about Type II silicon impression material are true EXCEPT_______________?
Found an error? Read our corrections policy and report it in the comments below.
A. They have a lower tear resistance than polysulphide rubbers
B. They exhibit a very low setting shrinkage
D. They evolve hydrogen when cast if they are not fully cured